Flap Assemblies, Rotary Flap Peening
Author: SAE
Source: SAE: AS2592
Doc ID: 2010033
Year of Publication: 2010
Abstract:
This standard was issued to cover equipment required to accomplish flap peening in accordance with AMS2590.
|
|---|
| For more information: http://www.sae.org |
|---|