Device and Method for the Surface Peening of a Component of a Gas Turbine
Author: Erwin Bayer; Max Niegl; Martin Bussmann; Thomas Peschke
Source: US Patent 8,931,318
Doc ID: 2015049
Year of Publication: 2015
Abstract:
A device for surface-peening, especially for the ultrasound shot-peening of a component of a gas turbine, having at least one vibration means that comprises a surface that propels the peening material, and having a holding means with which a surface area of the component and the surface of the vibration means can be arranged with respect to each other is disclosed. In this context, the angular position of the surface of the at least one vibration means can be adjusted relative to the surface area of the component of the gas turbine. Moreover, a method is provided in which he angular position of the surface of the at least one vibration means can be adjusted relative to the surface area of the component.