  • Measurement of Shot Peening Coverage by Correlation Analysis of Surface Line Data
  • Year: 1994, Source: US Patent 5,581,483
  • A method of measuring shot peening coverage includes correlation analysis of surface line data. The method comprises the use of cross correlation of two or more parallel profile traces of a shot peene...

  • Prestressed Brake Drum or Rotor
  • Year: 1994, Source: US Patent 5,664,648
  • Uniformly distributed compressive stresses are induced in the machined surfaces of brake drums and brake rotors. The compressive stresses cancel residual tensile stresses induced in the surfaces by ma...

  • Rotary Peening Tool
  • Year: 1994, Source: US Patent 5,727,995
  • A surface preparation tool for peening and removing a coating from a work surface, the tool including a rotating hub which retains plurality of peening flaps with peening particles attached at one end...

  • Spray Paint Monitoring and Control Using Doppler Radar Techniques
  • Year: 1994, Source: US Patent 5,315,306
  • Systems and methods that use a CW Doppler radar to monitor paint particle velocities as they are sprayed from a paint gun to optimize the application of strayed paint onto the object, and provide a cl...

  • Flow Regulating Valve for Magnetic Particles
  • Year: 1994, Source: US Patent 5,362,027
  • A valve for regulating the flow of matertials which are made up substantially of magnetic particles. The valve includes an outer housing and a core assembly secured within the housing to define an an...

  • Gage for Measuring the Intensity of Shot-Blast Peening
  • Year: 1994, Source: US Patent 5,297,418
  • An Almen type gage with an improved test strip support mechanism, which concentrates the holding force at the contact points. The support mechanism includes four paired contact balls and a permanent m...

  • Method for cleaning Surfaces with an Abrading Composition
  • Year: 1994, Source: US Patent 5,375,378
  • This invention relates to a method and devices for hydroblasting wherein a hydrolyzed solution of a silica compound and water, the hydrolyzed solution containing solid particles of the silica compound...

  • Less Aggressive Blast Media formed from Compacted Particles
  • Year: 1994, Source: US Patent 5,376,157
  • A blast media for stripping contaminants from very soft and sensitive substrates comprises compacted abrasive particles which are formed by compacting very fine particles of the abrasive into larger p...

  • Method of Improving the Surface of Steel Pipe for Corrosion Resistant Coating and Apparatus for use in Carrying out the Metho
  • Year: 1994, Source: US Patent 5,371,972
  • Surface anomalies on pipe are removed preparatory to corrosion coating. The removal is conducted by brusing with wire brush elements or Comax brush elements which may rotate about axes parallel to th...

  • Containing Structure for Abrasive Blast Head Rigging and Tank Side Cleaning Apparatus
  • Year: 1994, Source: US Patent 5,367,841
  • A protable containment structure for abrasive blasting equipment is designed for particular application in the cleaning of large stroage tanks and bor bridges. The unit includes a portable blasing ro...

  • Method and System for the Abrasive Cleaning of Surfaces.
  • Year: 1994, Source: US Patent 5,367,840
  • A system for abrasively cleaning surfaces such as by sandblasting and including a vacuum arrangement for recovering the material abrasively removed from the surface as well as the abrasive material is...

  • Particle Blasting using Crystalline Ice
  • Year: 1994, Source: US Patent 5,367,838
  • The invention relates to an improved method and apparatus for particle blasting utilizing crystalline ice. A theory of impact erosion is presented, as opposed to conventional abrasive techniques, whi...

  • Cleaning Method Utilizing Sodium Bicarbonate Particles.
  • Year: 1994, Source: US Patent 5,366,560
  • A method for effecting the continous reliable supply of sodium bicarbonate particles to a blasting nozzle employing pressured air or water as the means for conveying such particles into impact engagem...

  • Blast Cleaning System
  • Year: 1994, Source: US Patent 5,365,699
  • This invention relates to a carbon dioxide blast cleaning system for propelling dry-ice pellets by cryogens, manely high pressure nitrogen, helium and/or oxygen, against a surface being cleaned. Caar...


Previous     9   10   11   12   13   14   15   16   17       Next

The Shot Peener magazine

The Shot Peener magazine is dedicated to sharing information and expanding global markets for the shot peening and blast cleaning industries. We cover topics of importance to a wide range of readers -- from OEMs to engineers to academics to machine operators -- in a fresh and engaging format. The magazine is free of charge to make it accesssible to as large an audience as possible.

Electronics Inc. publishes the magazine. For more information, visit The Shot Peener magazine.

Sponsored by Electronics Inc. © 2026 Electronics Inc. All Rights Reserved.